Aluminium Alloy 7075 Datasheet

Aluminium Alloy 7075 Datasheet

Aluminium Alloy 7075 is capable of high strength as developed by heat treating. It also has excellent properties at low temperatures. It is amongst the strongest aluminium alloy with comparable strength to steel

Applications for Aluminium Alloy 7075
  • Aircraft fittings
  • Aerospace and defence applications
Chemical Compositions of Aluminium Alloy 7075
Element Composition %
Silicon (Si) 0.10 - 0.40
Iron (Fe) 0.10 - 0.50
Copper (Cu) 1.2 - 2.0
Manganese (Mn) 0.05 - 0.30
Magnesium (Mg) 2.10 - 2.90
Zinc (Zn) 5.10 - 6.10
Chromium (Cr) 0.15 - 0.28
Titanium (Ti) 0.01 - 0.20
Gallium (Ga) 0.01 - 0.05
Vanadium (V) 0.01 - 0.06
Aluminium (Al) Balance
Mechanical Properties of Aluminium Alloy 7075 - T651
Property Value
Proof Stress 440 Min MPa
Tensile Strength 572 MPa
Elongation at 50 mm 4 Min %
Hardness Brinell 155 HB
Please note that Mechanical Properties shown are for T651 temper
Aluminium Alloy 7075 Weldability
Gas Poor
Arc Poor
Brazability Poor
Resistance Excellent
Aluminium Alloy 7075 Fabrication
Machinability Good
Workability - Cold poor
Generic Physical Properties of Aluminium Alloy 7075
Property Value
Density 2.81 g/cm3
Melting Point 635°C
Thermal Expansion 23.6 ×10−6 /K
Modulus of Elasticity 72 GPa
Thermal Conductivity 130 W/m.K
Electrical Resistivity 0.0515 ×10−6Ω.m